DDP insulating paper

When the temperature rises to 90°C, the diamond paper begins to thaw all at once, and then solidifies all at once. When the temperature is maintained at 90°C for 90 minutes, the epoxy resin will safely bond to the adjacent cables and paper.

Classification:

keyword: Insulation material

  • Product Description
    • Commodity name: DDP insulating paper

    When the temperature rises to 90°C, the diamond paper begins to thaw all at once, and then solidifies all at once. When the temperature is maintained at 90°C for 90 minutes, the epoxy resin will safely bond to the adjacent cables and paper.

    Product Type: Diamond Dot Paper

    Color: Natural Color

    Diamond dot insulation paper is made of electrical insulation paper coated with thermosetting epoxy resin, with the epoxy resin adhesive applied to both sides of the paper, forming a diamond pattern of 9.5mm x 9.5mm.

    When the temperature rises to 90℃, the diamond paper begins to thaw once and then solidifies once. When the temperature is maintained at 90℃ for 90 minutes, the epoxy resin will safely adhere to the adjacent cables and paper.

    Thickness

    mm

    0.08

    0.13

    0.17

    0.20

    0.25

    0.30

    Thickness Tolerance

    %

    6.5

    Density

    g/cm3

    ≥0.85

    Tensile Strength

    MD

    7.5

    CD

    3.7

    Tear Strength

    m·N

    500

    1000

    1500

    2000

    Dielectric Loss

    KV

    0.6

    0.9

    1.2

    2.2

    2.75

    3.3

    Water Extract

    _

    6.8~8.5

    Adhesive Strength

    Kpa

    450

    Ash Content

    %

    1.0